(818) 773-8777
EP
FEATURES AND BENEFITS
PRODUCT SPCIFICATION
EP 48 Part A | Test Method | |
Color | Lt. Amber | Visual |
Viscosity, centipoise | 80 cps | ASTM D 2393 |
Specific Gravity, gms/cc | 1.18 | ASTM D1475 |
HANDLING PROPERTIES
Mixed Viscosity(cps) | 15,500 |
Work Life@ 770F(250C) | 60 minutes |
Demold Time@ 750-80F(240-27°C) | 16-24 hours |
EP 48 Parts B& B1 | Test Method | |
Color | Translucent | Visual |
Viscosity, centipoise | 900 cps | ASTM D 2393 |
Specific Gravity, gms/cc | 1.05 | ASTM D1475 |
EP49 Part A | Test Method | |
Color | Light Amber | Visual |
Viscosity, centipoise | 100 cps | ASTM D 2393 |
Specific Gravity, gms/cc | 1.10 | ASTM D1475 |
EP49 Parts B & B1 | Test Method | |
Color | Clear | Visual |
Viscosity, centipoise | 1300 cps | ASTM D 2393 |
Specific Gravity, gms/cc | 1.06 | ASTM D1475 |
TYPICAL MECHANICAL PROPERTIES
EP48A With B or B1
|
Test Method | ||
Rm. Temp. Cure | 1500 F Cure | ||
Working Time,4fl. oz. Mass, @770F | B: 6 min /B1: 12 min. | ASTM D2471 | |
Demold Time, 1/8″ sample @770F@1500F | B: 1 hour< 1 hour | B1: 2 hours < 2 hours |
PTM & W |
Peak Exotherm, 200 grams mass | B: 2400F / B1: 2110F | ASTM D2471 | |
Cured hardness, Shore D | 80-82 D | ASTM D2240 | |
Shrinkage, in/inMold#, Volume | B:0.002/ B1: 0.001 (Mold#0; 0.017 Gallon) |
ASTM D2566 | |
Specific Gravity, grams, cc | 1.11 | ASTM D1475 | |
Density, lb./cu. inchlb./gallon | .0402 9.2 |
ASTM D792 | |
Specific Volume, cu. in./lb. | 24.9 | ASTM D792 | |
Ultimate Tensile Strength, psi | 10,514 psi | 10,262 psi | ASTM D638 |
Elongation at Break, % | 7.2% | 7.5% | |
Tensile Modulus, psi | 381,615 psi | 357,765 psi | |
Ultimate Flexural Strength, psi | 14,438 psi | 14,800 psi | ASTM D790 |
Flexural Modulus psi | 390,911 psi | 369,110 psi | |
Compressive Strength, psi | 14,477 psi | 14,457 psi | ASTM D695 |
Compressive Modulus, psi | 418,977 psi | 393,170 psi | |
Glass Transition Temperature, Tg | 195oF | 207oF | TMA |
Thermal Coefficient of ExpansionRange:500C to 100oC | 5.26X 10-5in./in./0F | 6.11X 10-5in./in./0F | ASTM D696 |
Heat Deflection Temp., 66 psi264 psi | 130oF126oF | 166oF151oF | ASTM D 648 |
Izod Impact Strength, Notched(ft-lb.per inch of notch) Unnotched | 0.362.4 | 0.463.5 | ASTM D256 |
EP49A With B or B1
|
Test Method | ||
Rm. Temp. Cure | 1500F Cure | ||
Working Time,4fl. oz. Mass, @770F | B: 5-5 1/2 min /B1: 11-12 min | ASTM D2471 | |
Demold Time, 1/8″ sample @770F@1500F | B: 1 hour
< 1 hour |
B1: 2 hours
< 2 hours |
PTM & W |
Peak Exotherm, 200 grams mass | B: 2200F / B1: 2030F | ASTM D2471 | |
Cured hardness, Shore D | 70-75D | ASTM D2240 | |
Shrinkage, in/inMold#, Volume |
B:0.0015/ B1: 0.0009
|
ASTM D2566 | |
Specific Gravity, grams, cc | 1.08 | ASTM D1475 | |
Density, lb./cu. inchlb./gallon | .0392 9.07 |
ASTM D792 | |
Specific Volume, cu. in./lb. | 25.5 | ASTM D792 | |
Ultimate Tensile Strength, psi | 6,555 psi | 7,263 psi | ASTM D638 |
Elongation at Break, % | 6.6% | 7.6% | |
Tensile Modulus, psi | 267,600 psi | 238,110 psi | |
Ultimate Flexural Strength, psi | 9,428 psi | 10,253 psi | ASTM D790 |
Flexural Modulus psi | 274,424 psi | 244,498 psi | |
Compressive Strength, psi | 9,017 psi | 9,273 psi | ASTM D695 |
Compressive Modulus, psi | 288,613 psi | 276,097 psi | |
Glass Transition Temperature, Tg | 212oF | 216oF | TMA |
Thermal Coefficient of ExpansionRange:500C to 100oC | 9.97X 10-3in./in./0F | 7.4X 10-3in./in./0F | ASTM D696 |
Heat Deflection Temp., 66 psi264 psi | 134oF129oF | 175oF166oF | ASTM D 648 |
Izod Impact Strength, Notched(ft-lb.per inch of notch) Unnotched | 0.392.6 | 0.423.2 | ASTM D256 |